Product

 

 

For more information, please download the TDS available in PDF format below.BLUESIL RTV 3503 A may be stored at a temperature below 40 °C/ 104 °F for up to 12 months from its date of manufacturing.Please consult the Safety Data Sheet of this product.

BLUESIL RTV 3503 A

​BLUESIL RTV 3503 A&B is a two component silicone elastomer which cures at room temperature by a polyaddition reaction.

This reaction can be accelerated by heat.

Release

2 Part RTV

Fluid

  • High fluidity
  • Extreme softness
  • Good mechanical properties
  • Low linear shrinkage
  • No release of toxic substances during and after curing

 

​BLUESIL RTV 3503 A&B is specifically formulated to produce the silicone external layer of printing rollers, used for ceramic tiles printing application.

The product can find application also for general moldmaking, where a low hardness is required.

Asia Pacific;Central and South America;Europe Middle East Africa;North America

 Characteristics_A

 

 

ColorcolorlessPairedComp
Viscosity2000PairedCompmPa.s

 Characteristics_B

 

 

 

 

 Table_Characteristics_A_And_B

 

 

pot-life_0d649a54-7503-4c7c-a047-9d0c4b3e9f6apot-life_0d649a54-7503-4c7c-a047-9d0c4b3e9f6aPot life20PairedMixmin
hardness_cd523e03-72a3-4261-93f9-36f7bbeeafb1hardness_cd523e03-72a3-4261-93f9-36f7bbeeafb1Hardness3PairedMixsh.A

 

 

 

 

 

 

​Add 100 parts of BLUESIL RTV 3503 A to 100 parts of BLUESIL RTV 3503 B.

The two components may be intimately mixed either by hand or using a low-speed electric or pneumatic mixer to minimize the introduction of air into the mixture.

If no automatic equipment is available, then it is recommended to degas the mixed product in order to eliminate the air introduced during the mixing.

Be aware that contact with certain materials can inhibit the curing of this RTV:

  • Natural rubbers vulcanized with Sulphur,
  • Polycondensation RTV catalyzed with metal salts,
  • PVC stabilizing agents,
  • Amine cured epoxies,
  • Sulphur containing clays.

If doubts exist it is recommended to run a quick test with a small quantity of material in order to assess compatibility. Take duly note that the cross contamination due to not well cleaned tools or devices is frequently the main cause of inhibition. The best way is to use only dedicated gear when processing polyaddition RTVs.

​Add 100 parts of BLUESIL RTV 3503 A to 100 parts of BLUESIL RTV 3503 B.The two components may be intimately mixed either by hand or using a low-speed electric or pneumatic mixer to minimize the introduction of air into the mixture. If no automatic equipment is available, then it is recommended to degas the mixed product in order to eliminate the air introduced during the mixing.Be aware that contact with certain materials can inhibit the curing of this RTVNatural rubbers vulcanized with Sulphur,Polycondensation RTV catalyzed with metal salts,PVC stabilizing agents,Amine cured epoxies,Sulphur containing clays.If doubts exist it is recommended to run a quick test with a small quantity of material in order to assess compatibility. Take duly note that the cross contamination due to not well cleaned tools or devices is frequently the main cause of inhibition. The best way is to use only dedicated gear when processing polyaddition RTVs.

 

 

​Add 100 parts of BLUESIL RTV 3503 A to 100 parts of BLUESIL RTV 3503 B.

The two components may be intimately mixed either by hand or using a low-speed electric or pneumatic mixer to minimize the introduction of air into the mixture.

If no automatic equipment is available, then it is recommended to degas the mixed product in order to eliminate the air introduced during the mixing.

Be aware that contact with certain materials can inhibit the curing of this RTV:

  • Natural rubbers vulcanized with Sulphur,
  • Polycondensation RTV catalyzed with metal salts,
  • PVC stabilizing agents,
  • Amine cured epoxies,
  • Sulphur containing clays.

If doubts exist it is recommended to run a quick test with a small quantity of material in order to assess compatibility. Take duly note that the cross contamination due to not well cleaned tools or devices is frequently the main cause of inhibition. The best way is to use only dedicated gear when processing polyaddition RTVs.

​Add 100 parts of BLUESIL RTV 3503 A to 100 parts of BLUESIL RTV 3503 B.The two components may be intimately mixed either by hand or using a low-speed electric or pneumatic mixer to minimize the introduction of air into the mixture. If no automatic equipment is available, then it is recommended to degas the mixed product in order to eliminate the air introduced during the mixing.Be aware that contact with certain materials can inhibit the curing of this RTVNatural rubbers vulcanized with Sulphur,Polycondensation RTV catalyzed with metal salts,PVC stabilizing agents,Amine cured epoxies,Sulphur containing clays.If doubts exist it is recommended to run a quick test with a small quantity of material in order to assess compatibility. Take duly note that the cross contamination due to not well cleaned tools or devices is frequently the main cause of inhibition. The best way is to use only dedicated gear when processing polyaddition RTVs.